Metal ceramic veneering powder for noble and non-precious alloys with a coefficient of thermal expansion (CTE) of 13.8-15.4 μm/m. Part of the Duceram Kiss simplified layering system that reduces the number of required powders by nearly half compared to conventional ceramic systems. Features excellent color stability through advanced pigmentation philosophy and supports rapid firing programs up to 80°C/min with fast cooling. Package contains 1 jar of 75g.